-40%

Brazing Alloy, Lucas Milhaupt, Handy Flo, 8 Rods

$ 17.22

Availability: 87 in stock
  • Brand: Lucas-Milhaupt, Inc.
  • Type: Handy Flo
  • Country of Manufacture: United States
  • MPN: 95136
  • Model: brazing alloy
  • Condition: New

    Description

    Gregoriou Brothers Refrigeration Since 1979
    Frosty-Freeze
    Brazing Alloy, Lucas Milhaupt, Handy Flo, 8 Rods
    Made by Lucas-Milhaupt, Inc.
    A Handy & Harman Company
    Part# 95136
    Handy-Flo
    For Joining Copper and Copper-based Alloys.
    6% Ag.
    .125" x .050" x 20" Long
    8 Rods
    For joining copper to copper without a flux and copper based alloys (brass and bronze) with a flux.
    This brazing alloy has been developed and patented for over 75 years.
    Sil-Fos is the "WORKHORSE" filler metal used in the refrigeration and air conditioning industry.
    Think of the brazing alloy as the glue that holds the refrigeration system together.
    The thermal cycling (and subsequent expansion and contraction), vibration stresses and higher pressures of the new refrigerants like (R-410A) strongly suggest that the ductility of the braze alloy is extremely important.
    Not just for an initial leak tight joint, but to be hermetic (sealed) for many years down the road.
    Ag: 6%
    Cu: 88%
    P: 6%
    Melt: 1190 F.
    Flow: 1460 F.
    $Made by Lucas-Milhaupt, Inc. A Handy & Harman Company Part# 95136 Handy-Flo For Joining Copper and Copper-based Alloys. 6% Ag. .125" x .050" x 20" Long 8 Rods For joining copper to copper without a flux and copper based alloys (brass and bronze) with a flux. This brazing alloy has been developed and patented for over 75 years. Sil-Fos is the "WORKHORSE" filler metal used in the refrigeration and air conditioning industry. Think of the brazing alloy as the glue that holds the refrigeration system together. The thermal cycling (and subsequent expansion and contraction), vibration stresses and higher pressures of the new refrigerants like (R-410A) strongly suggest that the ductility of the braze alloy is extremely important. Not just for an initial leak tight joint, but to be hermetic (sealed) for many years down the road. Ag: 6% Cu: 88% P: 6% Melt: 1190 F. Flow: 1460 F.
    Gregoriou Brothers Refrigeration Since 1979
    Frosty-Freeze
    Brazing Alloy, Lucas Milhaupt, Handy Flo, 8 Rods
    Made by Lucas-Milhaupt, Inc.
    A Handy & Harman Company
    Part# 95136
    Handy-Flo
    For Joining Copper and Copper-based Alloys.
    6% Ag.
    .125" x .050" x 20" Long
    8 Rods
    For joining copper to copper without a flux and copper based alloys (brass and bronze) with a flux.
    This brazing alloy has been developed and patented for over 75 years.
    Sil-Fos is the "WORKHORSE" filler metal used in the refrigeration and air conditioning industry.
    Think of the brazing alloy as the glue that holds the refrigeration system together.
    The thermal cycling (and subsequent expansion and contraction), vibration stresses and higher pressures of the new refrigerants like (R-410A) strongly suggest that the ductility of the braze alloy is extremely important.
    Not just for an initial leak tight joint, but to be hermetic (sealed) for many years down the road.
    Ag: 6%
    Cu: 88%
    P: 6%
    Melt: 1190 F.
    Flow: 1460 F.
    Made by Lucas-Milhaupt, Inc.
    A Handy & Harman Company
    Part# 95136
    Handy-Flo
    For Joining Copper and Copper-based Alloys.
    6% Ag.
    .125" x .050" x 20" Long
    8 Rods
    For joining copper to copper without a flux and copper based alloys (brass and bronze) with a flux.
    This brazing alloy has been developed and patented for over 75 years.
    Sil-Fos is the "WORKHORSE" filler metal used in the refrigeration and air conditioning industry.
    Think of the brazing alloy as the glue that holds the refrigeration system together.
    The thermal cycling (and subsequent expansion and contraction), vibration stresses and higher pressures of the new refrigerants like (R-410A) strongly suggest that the ductility of the braze alloy is extremely important.
    Not just for an initial leak tight joint, but to be hermetic (sealed) for many years down the road.
    Ag: 6%
    Cu: 88%
    P: 6%
    Melt: 1190 F.
    Flow: 1460 F.